First layer not sticking? Improve your 3D print systematically

Applies to: Bambu Lab P1S, A1 · Bambu Studio · PLA, PETG · table for Bambu Textured PEI Plate

PLA or PETG not sticking to the build plate? Check the surface, plate profile, calibration and first print lines.

By Yener Karayel · Published by: YK Design & Print · Published on · Updated on · Free, no registration required

Yener’s Bambu Studio screenshot: first layer 50 mm/s and first-layer infill 60 mm/s
Slicer screenshot from Yener’s reel. The values show Yener’s example profile. Open the original video
The short answer

First check the actual build plate and material profile. Clean according to the plate's instructions and check the intended bed calibration. Then observe a small first-layer test before changing temperature, speed or flow.

Open the relevant troubleshooting helper

Could this help someone else too? Share the free guide.

How do you recognise the problem?

Lines lift immediately, get dragged along by the nozzle or have gaps. An overly squashed, rough first layer also indicates unsuitable printing conditions.

What you observeWhat could be behind itYour next step
Rounded lines with spaces between themNozzle distance or material deposition may be unsuitable.Check calibration and profile.
Rough, translucent or ridged layerThe lines may be squashed too much.Cancel the print if the nozzle scrapes the plate.
Only one area has poor adhesionLocal residue or an uneven surface may be responsible.Check the plate with a test spread across its surface.

Aus meinem eigenen Beitrag

First layer: Kontur und Füllung unterscheiden.

Im Video ändere ich das Feld „Füllung der ersten Schicht“ von 105 to 60 mm/s. Das separate Feld „First layer“ bleibt im gezeigten Profil bei 50 mm/s. Die Ausschnitte machen den Unterschied sichtbar.

Bambu Studio vor der Change: First layer 50 mm/s, Füllung der ersten Schicht 105 mm/sBild vergrößern
Vor der Change: First layer 50 mm/s; Füllung 105 mm/s.
Bambu Studio nach der Change: First layer 50 mm/s, Füllung der ersten Schicht 60 mm/sBild vergrößern
Nach der Change: First layer weiterhin 50 mm/s; Füllung 60 mm/s.

Im Screenshot ist ein Bambu Lab P1S mit 0,4-mm-Düse ausgewählt. Die sichtbare Change betrifft die Füllung. Aus dieser Menüänderung allein lässt sich noch keine gemessene Verbesserung der Adhesion ableiten.

Das Example mit Prüfschritten ansehen

Possible causes

  • Residue on the print surface
  • Wrong build plate selected in the slicer
  • Incorrect nozzle distance or faulty calibration
  • Unsuitable temperature or excessive initial speed

Narrow it down step by step

Change one thing at a time and compare using the same small test print. Check off the steps you have completed.

0 of 6 steps checked

  1. Match the plate and material

    Check the plate type in the slicer and its suitability for your material. Smooth PEI, textured PEI and specialty plates have different cleaning and temperature requirements.

  2. Clean the surface appropriately

    Remove residue using the method recommended by the plate manufacturer. Avoid touching the print surface with your skin. An adhesive or release agent is useful only if it is compatible with the plate and filament.

  3. Check the nozzle tip

    Material residue can interfere with probing or startup. Use the intended cleaning procedure. Do not touch the hot nozzle, and protect the plate from unsuitable tools.

  4. Check bed calibration

    Perform the automatic or manual calibration intended for your printer. Do not change a manual Z offset indiscriminately: some printers determine the height automatically and need a different checking procedure.

  5. Observe a small surface test

    Adjacent paths should meet evenly. Watch the start and stop if scraping or lifting occurs. Compare different areas of the plate to identify local problems.

  6. Only then fine-tune the start

    Once the plate and calibration are correct, test a lower first-layer speed within your profile's limits. Start by changing just one parameter. Higher flow does not replace a properly prepared surface.

First layer in Bambu Studio

Before slicing, check the selected printer, nozzle, filament and build plate. First-layer speed is a separate setting. A slower start can help, but it will not fix an incorrect plate selection. Use automatic calibration according to the guidance for your Bambu model.

Bed and nozzle temperatures for the first layer

Identify your build plate first. The bed ranges below apply to Bambu's textured PEI plate; Cool Plate, SuperTack and smooth plates require their own settings.

Manufacturer ranges for Bambu Textured PEI Plate and the example filaments listed.
MaterialNozzle temperatureBed · Textured PEIWhat to check
PLA · example: Bambu PLA Basic190–230 °C45–60 °CLoad the matching plate profile. On an enclosed P1S, follow the manufacturer's PLA heat-management guidance.
PETG · example: Bambu PETG HF230–260 °C60–80 °CDo not transfer these bed values to smooth PEI. Follow manufacturer instructions for adhesives or release agents.

Reference values; the filament manufacturer's specifications take priority.

Within these ranges, use the profile for your actual filament, plate and nozzle. Do not change nozzle temperature, bed temperature and speed together. If specifications differ, the instructions for your particular filament and plate take priority. The figures are manufacturer specifications, not our own comparative measurements.

Sources: Bambu Lab: PLA Basic technical data sheet · Bambu Lab: PETG HF printing and drying settings · Bambu Lab: Textured PEI Plate temperature recommendations · checked on

Your next comparison print

Platte und Profil prüfen, bevor du Zubehör kaufst

Halte Plattentyp, Material, Düsen- und Betttemperatur sowie die Geschwindigkeit des ersten Layers fest. Vergleiche zuerst das unveränderte Herstellerprofil. Fotografiere dieselbe Stelle des kleinen Testdrucks vor und nach genau einer Change.

Für reine Haftungsprobleme ist ein Neukauf nicht der erste Check.

Open the free test logA test plan for your own trial. The illustration above is an example; documented results from your printer come from the actual test.
VIDEO GUIDE BY YENER

First layer: compare speeds systematically

In diesem Reel ändert Yener das Feld „Füllung der ersten Schicht“ von 105 to 60 mm/s. Das separate Feld „First layer“ bleibt im gezeigten Profil bei 50 mm/s. Die Werte gehören zu diesem Example und sind keine allgemeine Vorgabe.

Watch the linked Reel here or open it directly on Instagram.

Clicking loads content from Instagram (Meta). Data such as your IP address is transmitted to Meta; Instagram may use cookies and similar storage. Privacy policy

Watch the video on Instagram →

Slicer and material

These settings matter

  • Use the correct plate and filament profile
  • Check temperatures against plate and material approvals
  • Test first-layer speed separately
  • Add a brim only with a suitable contact surface

PETG can adhere too strongly to some smooth surfaces. A prescribed release layer also protects the plate in these cases. Stronger adhesion is not the goal under every condition.

Frequently asked questions

Should I always use adhesive spray?

No. Suitability depends on the plate and material. First check the instructions and establish a clean starting condition.

Why does PLA lift despite a slow first layer?

Possible causes include residue, an incorrect plate profile or unsuitable height calibration. Speed is only one part of the process.

What bed temperature does PLA need on Bambu Textured PEI?

The linked plate recommendation specifies 45–60 °C for PLA. Choose the profile for your filament and check the actual plate type. Cool Plate and SuperTack have different requirements.

What bed and nozzle temperatures does PETG need?

For Bambu PETG HF, the manufacturer specifies a nozzle temperature of 230–260 °C. The textured PEI plate covered here specifies a bed temperature of 60–80 °C for PETG. Other PETG types or plates require their own specifications.

Should I change the Z offset on a Bambu P1S or A1?

First check the plate, a clean nozzle tip, the profile and the prescribed bed calibration. Do not copy a manual Z correction from another printer model; height detection depends on the model.

How do I recognise a good first layer?

Adjacent lines form a continuous surface and stay on the plate. Round separated lines, raised ridges or scraping are reasons to recheck the start. A small patch test is quicker to compare than a large print.

Related guides for further reading

Compare all 15 printing defects

Manufacturer information and further sources

This sequence of checks puts typical symptoms into context. Specific maintenance procedures always apply to the respective printer model.

Applies to FDM/FFF printing with filament. No automatic photo analysis. For hot, electrical or moving components, follow the manufacturer's safety and maintenance instructions.