Fix under-extrusion in 3D printing

Gaps in walls or thin layers? Check the filament path, nozzle and volumetric flow step by step before changing the flow setting.

By Yener Karayel · Published by: YK Design & Print · Published on · Updated on · Free, no registration required

Under-extrusion & gaps: Interrupted print lines leave visible gaps in a plastic wall. AI-generated example.
AI example image
AI-generated example image · not a documented print test. The feature offers a clue; the cause is checked step by step.
The short answer

Start with the correct printer, nozzle and filament profiles. Then check the spool and the entire filament path. Only once feeding and the nozzle work properly is it worth testing a lower volumetric flow and calibrating flow.

Open the relevant troubleshooting helper

Could this help someone else too? Share the free guide.

How do you recognise the problem?

Your print has gaps, individual lines are missing or the wall looks thinner than in the preview. The extruder may also click. This symptom indicates that too little material is being deposited; it does not yet identify the cause.

What you observeWhat could be behind itYour next step
Gaps appear only in fast sectionsThe required material throughput may be too high.Compare at a lower speed using the appropriate standard profile.
Feeding also falters during extrusionThe filament path, extruder or hotend may be obstructed.Check feeding, then follow the model-specific maintenance instructions.
Only the first layer has gapsThe build plate, height measurement or first layer may be the cause.Use the first-layer guide.

Possible causes

  • Resistance at the spool, AMS or filament guide
  • Partially blocked nozzle or dirty extruder
  • More material requested than the hotend can melt
  • Unsuitable profile or damp filament

Narrow it down step by step

Change one thing at a time and compare using the same small test print. Check off the steps you have completed.

0 of 6 steps checked

  1. Record the starting conditions

    Record the printer, nozzle diameter, material and affected layers. Compare the area with the slicer preview: increasing flow will not fix a missing model wall or geometry designed too thin.

  2. Load the correct profile

    For comparison, use an unmodified profile for your actual nozzle and material. Also check the filament diameter. A profile for a different nozzle can request incorrect material quantities even without a hardware fault.

  3. Check the spool and material path

    Watch for a spool that does not turn freely, crossed filament or a sharply bent tube. With an AMS, include its feed path. If an error message appears, first work through the manufacturer's procedure for that error.

  4. Compare with known-good material

    A short test with a spool that prints reliably helps distinguish material issues from machine issues. Damp, brittle or heavily ground filament can disrupt feeding. Note which spool you actually tested.

  5. Check the extruder and hotend systematically

    If the feed path is clear but material is still missing, follow the manufacturer's instructions to check the extruder, hotend cooling and possible partial clogs. Opening and cleaning procedures differ between printer models.

  6. Test throughput, then calibrate flow

    Compare a small print at a reduced volumetric flow. If it prints cleanly, investigate the interaction between speed, material and melting capacity. Fine-tune flow only once feeding is stable and printing conditions are suitable.

Gaps in the first layer or throughout the print?

If the upper layers are solid, start with the first-layer guide. If gaps also appear in walls and upper layers, check the filament feed and volumetric flow. If no material exits the nozzle during loading, follow the clogged-nozzle guide.

Under-extrusion with Bambu Lab and Bambu Studio

In Bambu Studio, check the selected printer model, installed nozzle and filament profile. Flow Ratio, Flow Dynamics and maximum volumetric speed serve different purposes. Do not increase all three at once. If there are AMS problems, feeding must work reliably first. Comparing an unmodified profile is more informative than collecting untested values from other setups.

How to assess your comparison print

For each comparison, use the same small model, orientation and material. Change only one setting and photograph the same area. Compare closed walls, consistent lines and layer adhesion. A better-looking top surface alone does not prove that overall material flow is correct.

Your own comparison

Is material already missing during feeding, or only at high throughput?

Record the starting point
Note whether feeding stalls during the intended loading procedure or gaps appear only in certain areas of the print.
Check deliberately
If the feed path is clear and loading is normal, compare the same small print with a lower maximum volumetric flow. Leave flow unchanged for now.
Assess afterwards
Mark the same wall areas and compare line continuity. A better print at lower throughput is a clue for further checks, not yet proof of a faulty nozzle.

This is a troubleshooting guide for your own print. Document your observations so you can find effective changes again.

Use the test log and free template →

Slicer and material

These settings matter

  • Use the correct printer, nozzle and material profile as a reference
  • Reduce maximum volumetric speed on its own and compare
  • Test temperatures only within the material and printer's approved limits
  • Fine-tune Flow Ratio only once feeding works reliably

PLA, PETG, silk and filled filaments can require different melting capacities at identical speeds. Do not copy a high volumetric flow from another spool without checking it.

Frequently asked questions

Should I simply increase flow for under-extrusion?

Check the profile, filament transport and hotend first. Higher flow can mask a mechanical issue and cause excess material elsewhere.

Why does under-extrusion start only after a longer printing time?

Possible causes include changing spool resistance, a blockage developing or a thermal issue at the hotend. Record when feeding weakens and check the fan according to the manufacturer's instructions.

Does under-extrusion always mean a clogged nozzle?

No. Profiles, material feeding and excessive throughput are also possible causes. For example, a new nozzle will not remove resistance at the spool.

Related guides for further reading

Compare all 15 printing defects

Manufacturer information and further sources

This sequence of checks puts typical symptoms into context. Specific maintenance procedures always apply to the respective printer model.

Applies to FDM/FFF printing with filament. No automatic photo analysis. For hot, electrical or moving components, follow the manufacturer's safety and maintenance instructions.